Sputtering Pyrex
2001-08-29
Robert D White
2001-08-29
Luesebrink Helge
Sputtering Pyrex
Luesebrink Helge
2001-08-29
Robert,

Did you try Si/Pyrex/Si triple stack anodic bonding using a pyrex wafer
instead of sputtering pyrex?

More info is at http://www.sensorsmag.com/articles/1298/sil1298/main.shtml


Scroll down to "Advanced Wafer Bonding"

Regards,
Helge


                -----Original Message-----
                From:   Robert D White [mailto:[email protected]]
                Sent:   Wednesday, August 29, 2001 3:09 PM
                To:     [email protected]
                Subject:        [mems-talk] Sputtering Pyrex

                MEMS Researchers,

                I am considering anondic bonding of two silicon wafers by
first
                sputtering pyrex onto one wafer.
                Does anyone know of a group who will sputter pyrex?

                Thanks,

                Robert White
                University of Michigan


                _______________________________________________
                mems-talk mailing list
                [email protected]
                To unsubscribe or change your list options, use:
                 http://fab.mems-exchange.org/mailman/listinfo/mems-talk


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
The Branford Group
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.