SU8 removal
2001-09-19
Browning, R (Richard)
SU8 removal
Browning, R (Richard)
2001-09-19
We are removing SU8 from copper structures
High temperatures are causing a differential expansion problem.
Does anyone have a method of removing SU8 at room temperature which does not
remove the copper as well

Thank You
Richard Browning