MEMSnet Home: MEMS-Talk: Re: processing information wanted
Re: processing information wanted
1996-05-29
Mike Gibbs
1996-06-09
Gang Lin
1996-06-10
Pierre Jaccard
1996-06-15
[email protected]
Re: processing information wanted
Mike Gibbs
1996-05-29
In response to the request for processing information on to polyimide

We have successfully sputter deposited a range of transition metals and
transition metal alloys onto Kapton with good adhesion. The substrate is
dgreased using standard solvents, and only given a very short sputter clean
before growth.

Maximum thickness we have tried is 1 micron.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Nano-Master, Inc.
MEMStaff Inc.
Tanner EDA by Mentor Graphics