Hello,

I have a couple of questions with regard to laser drilling of ceramics:

- during laser drilling, we have observed black spots around the drilled
holes, I am curious to know where do they originate from (earlier it was
believed that the emulsitone that was applied onto the  ceramic prior to
drilling lead to carbon deposits, but I find it hard to believe that carbon
doesnt get oxidized at high temperatures in an oxygen environment).
- secondly is there anyway to remove slags around the holes during the
drilling operation (say for e.g. by using coolants etc.), this is a concern
because when we remove the slag after the drilling operation by scrubbing,
we leave the substrate with plenty of scratches, so ideally I would like to
remove the slag as and when they are formed.

Thank you for your patience.
Regards,
Adnan Merhaba
Thin film process engineer
American Technical Ceramics
Jacksonville, Florida

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Addison Engineering
University Wafer