In microelectronics, pad ox. generally refers to a thin thermal oxide layer
used as a stress compliance layer underneath LPCVD silicon nitride, when the
nitride is deposited onto silicon. An example is nitride used as a hardmask
for Si trench etch. Apparently, the silicon surface is in better shape after
stripping the hardmask, if a oxide has been used as a buffer. Since trench
etch is pre-gate oxide, the silicon surface quality is critical. It is
generally stripped with BOE (Buffered Oxide Etch).

Best regards,

David Kinosky
Reveo, Inc.
3 Westchester Plaza
Elmsford, NY 10523


-----Original Message-----
From: [email protected]
[mailto:[email protected]]
Sent: Thursday, October 11, 2001 12:01 PM
To: [email protected]
Subject: mems-talk digest, Vol 1 #67 - 1 msg


Send mems-talk mailing list submissions to
        [email protected]

To subscribe or unsubscribe via the World Wide Web, visit
        http://fab.mems-exchange.org/mailman/listinfo/mems-talk
or, via email, send a message with subject or body 'help' to
        [email protected]

You can reach the person managing the list at
        [email protected]

When replying, please edit your Subject line so it is more specific
than "Re: Contents of mems-talk digest..."


Today's Topics:

   1. Pad etch (Karen Smith)

--__--__--

Message: 1
From: "Karen Smith" 
To: [email protected]
Date: Wed, 10 Oct 2001 17:18:53 +0000
Subject: [mems-talk] Pad etch

I have seen several references to "Pad etch" in
micromachining literature - specifically relating to
removal of a sacrificial oxide layer.

I have asked several chamical suppliers and checked
in several references to  no avail (I believe it
is a specialisat formulation (HF?) by Ashland, but
can find no reference to it on their MSDS?).

Can anyone help me with what it actually is & who
supplies it?

Best regards,

Karen Smith
MST consultant
Coventry, UK

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp


--__--__--

_______________________________________________
mems-talk mailing list
[email protected]
http://fab.mems-exchange.org/mailman/listinfo/mems-talk


End of mems-talk Digest

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
University Wafer
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing