A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: ion imlant depth vs energy for As, B, etc
photoresist heat capacity
2001-11-05
Andrey Bayrashev
ion imlant depth vs energy for As, B, etc
2001-11-06
jaideep mavoori
2001-11-08
Sonia Garcia Blanco
ion imlant depth vs energy for As, B, etc
Sonia Garcia Blanco
2001-11-08
Dear Jaideep,

You can try the software TRIM that simulates the penetration of ions of
different energies on different materials by MonteCarlo simulations.

I think you can find it on the Web....

Good luck!

Sonia.

*****************************************************

Sonia Garcia-Blanco

Department of Electronics and Electrical Engineering
University of Glasgow
Oakfield Ave.
G12 8LT
Glasgow

Phone:
   Office: (0141) 339 8855 ext 0101
   Lab:    (0141) 330 6014
Email: [email protected]

****************************************************

On Mon, 5 Nov 2001, jaideep mavoori wrote:

> Hello.
> Is there a table/software for calculating ion implant depth vs energy for
> various tilt angles for various species and substrates (Si primarily).
>
> Thanks.
> Jaideep
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
MEMS Technology Review
University Wafer
Addison Engineering