etching stainless steel
2001-11-09
John Somerville
etching stainless steel
John Somerville
2001-11-09
Does anyone have any good recipies for etching stainless suitable for a
depth of 100 microns or so (i.e. not to slow), I'm trying to avoid surface
pitting and would rather not use electrochemical etches.

Regards
John

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Mentor Graphics Corporation
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing