Measurements
Dear Steve: Resist parameters of Shipley are in IntelliFAB software or in the
Fabrication Database of IntelliCAD. For further info call one of our software
engineers and they will assist you in giving you the parameters that you need.

Regards,

Fariborz Maseeh
IntelliSense Corporation
(508) 988 - 8000
(508) 988 - 8001 fax


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.