Dear MEMS experts,

I 'm looking for information about pyrex deep etching.
Actually, we would like to realize some cicular micro-covers starting
from a pyrex wafer.
These covers have a diameter of around 2 mm.
Could you give me any information about a suitable technique for this
kind of operation?

Thanks a lot.


--
**********************************************
Dr. Paolo Bondavalli
R&D Engineer
LABCOM - Laboratoire Interconnexions Optiques et MEMS
THALES (ex THOMSON-CSF) CORPORATE RESEARCH CENTER
Domaine de Corbeville,
Route Departementale 128
F91404 ORSAY
(FRANCE)
Tel : 01 69 33 08 63
Fax : 01 69 33 08 62
Email : [email protected]
**********************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
University Wafer