MEMSnet Home: MEMS-Talk: Quality improvement of backside oxide of silicon wafer
Quality improvement of backside oxide of silicon wafer
2001-11-26
Soumen Das
Quality improvement of backside oxide of silicon wafer
2001-11-27
Kenneth Smith
Quality improvement of backside oxide of silicon wafer
Kenneth Smith
2001-11-27
if you are looking to have an even etch rate on both sides, the best
solution to your problem  is to use wafers with both sides of wafer
polished so that the surface roughness is similar. This would be easier
than trying to manage the oxide thickness or change the oxide methods (
compensating with higher thickness oxide on back)
If the base wafers are single side polished with a KOH etch backside and
depending on the lapping compound and the original etch method/process
(time/temp), the backside will be extremely rough reducing the oxide
thickness uniformity on the back. With your controlled etch of the front
side, the high points (low oxide) areas of the back will etch through
much faster.
Another base wafer alternative would be to use a good a acid etched
substrate instead of a caustic etched one. The problem here is obtaining
acid etch wafers which fewer suppliers can provide and this will only
improve, but still not be as good as using double side polished wafers.

Ken

Soumen Das wrote:
>
> Hello
> We are doing the silicon etching through windows simultaneously from both,
> front and back sides using KOH solution. The masking material for silicon
> etching is thermally grown 1 micron thick silicon dioxide. We observed that
> front side oxide remains for very long time in KOH soluton. However, back side
> oxide does not stay for long time. It etch out very fast than front side
> oxide.
> The wafer backside roughness is much higher than frontside surface. How can we
> improve the backside oxide quality to be used as masking material for KOH
> etching
> Do anyone has any solution?
> Thanks
> Dr. Soumen Das
> Sr. Scientific Officer
> Microelectronics Centre
> Dept. of Electronics & ECE
> Indian Institute of Technology
> Kharagpur 721 302, India
> email: [email protected]
> Phone: +91-3222-81914 (O)
>             +91-3222-81475 (Lab)
>             +91-3222-81915 (R)
> Fax: +91-3222-755303/777190
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

--


Kmbh Associates
4968 Charter Road
Rocklin, CA  95765  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG,
SOS.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation