A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: plasma chemistry for E-glass etching
plasma chemistry for E-glass etching
2001-12-07
Robert Dean
2001-12-07
martin.walker4
2001-12-07
[email protected]
2001-12-08
[email protected]
2001-12-11
Jon Doe
any hydrophillic layer?
2001-12-11
jung hoon yeom
2001-12-12
Helen Berney
2001-12-11
[email protected]
plasma chemistry for E-glass etching
[email protected]
2001-12-08
I have a new design that I would like your collective opinion on. First off
how much of the MEMS work that is currently being done or will in the near
future require etching of quartz pyrex or soda lime glass? Can anyone
determine the range of etch depth requirements? I understand from talking
with some MEMS engineers that 3 microns depth on pyrex or glass substrates is
required. Also, does the profile of the etch need to be anisotropic is would
a 60-70 degree slope be preferable for step coverage? If a slope is required
would a wet etch with a 2% uniformity across the wafer be acceptable? My
proposed design would provide the above results in a single wafer etch
design. Since we build production equipment our ultimate design would do
multiple wafers at a time for increased throughput. Does this process merit
serious consideration and would anyone be interested in pursuing this process
with us? Let me know

Bob Henderson
Process Integration,LLC
75 W. Baseline Rd. Suite E-32
Gilbert, Arizona 85233
Phone: 480-558-1156
Fax: 480-558-1161
email: [email protected]

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Addison Engineering
Nano-Master, Inc.
Tanner EDA by Mentor Graphics