I did 1000A.

Yh


>From: Satej Chaudhary 
>To: [email protected]
>Subject: [mems-talk] wire bonding on Ti Au
>Date: Wed, 5 Dec 2001 15:21:09 -0800 (PST)
>
> > Hi,
> >
> > I would like to know what is the minimum thickness
> > of the upper gold layer on a
> > Ti/Au pad in order to proceed to a wire bonding
> > without any risk?
>
>0.5 microns is the standard way to go i have heard
>though i havnt tried it myself.
>satej
>Grad student University of Maryland
>Send your FREE holiday greetings online!
>http://greetings.yahoo.com
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://fab.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/


_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics