Hi
You probably need a thin layer of Cr ( even stainless steel) between Pd and
Glass.

Vladimir
Nayna Networks

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Rajsekhar Popuri
Sent: Friday, December 07, 2001 7:09 AM
To: [email protected]
Subject: [mems-talk] lift-off


Hello,

I am trying to do a lift-off.I sputter coated gold-palladium of 2000A
thickness on a glass wafer.When i tried to do a lift-off with
acetone-methanol,gold-palladium layer was completely peeled off the glass
wafer.Can anyone tell me the reason for this and suggest a suitable process
to do a lift-off with gold-palladium.

Thanks in advance
Rajsekhar.




_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Mentor Graphics Corporation
Harrick Plasma, Inc.
University Wafer