A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: bonding silicone rubber or PMMA with Si or poly-Si
bonding silicone rubber or PMMA with Si or poly-Si
2001-12-11
Ebin Liao
bonding silicone rubber or PMMA with Si or poly-Si
2001-12-12
Heiko van der Linden
bonding silicone rubber or PMMA with Si or poly-Si
2001-12-12
Jeff Zahn
bonding silicone rubber or PMMA with Si or poly-Si
Heiko van der Linden
2001-12-12
Hi Ebin,

I know that PDMS ( a silicone rubber, SYLGARD 194) can be bonded with
good results to silicon, silicon oxide, glassy carbon, etc.you have to
oxidize the top layer of the PDMS in an O2 plasma. The surface will then
contain oxide groups that will condense with for instance silicon oxide
thus resulting in a very strong bond. Try to find the article by
Whitesides and Duffy about microstructuring in PDMS. There you can read
all the details.

Good luck,

Heiko van der Linden

*******************************
MESA+ Research Institute
      Twente University
         P.O. Box 217
     7500 AE Enschede
       The Netherlands
*******************************


-----Original Message-----
From: [email protected] [mailto:[email protected]]
On Behalf Of Ebin Liao
Sent: Wednesday, December 12, 2001 5:50 AM
To: [email protected]
Subject: [mems-talk] bonding silicone rubber or PMMA with Si or poly-Si


Dear All:

I have made a micromachined sensor chip, and now I'd
like to bond it (Si or Poly-Si) to some polymeric
slices (silicone rubber or PMMA). Someone told me it
was very difficult to bond silicone rubber with other materials. Anyone
has experience for bonding silicone rubber or PMMA to Si or poly-Si? I'd
like to try Super Glue by hand at first. Anyone has other suggestions?
Thanks a lot.

Best regards,

Ebin
Check out Yahoo! Shopping and Yahoo! Auctions for all of
your unique holiday gifts! Buy at http://shopping.yahoo.com
or bid at http://auctions.yahoo.com
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
MEMS Technology Review
Tanner EDA by Mentor Graphics
The Branford Group