MEMSnet Home: MEMS-Talk: [memstalk] SOS wafer
[memstalk] SOS wafer
[memstalk] SOS wafer
2001-12-12
Carl Kubler
[memstalk] SOS wafer
2001-12-13
John Somerville
[memstalk] SOS wafer
2001-12-13
tom_wester
Thick PSG
2001-12-13
Jon Doe
2001-12-14
Michael Pedersen
2001-12-14
Jon Doe
2001-12-14
Michael Pedersen
2001-12-14
Helen Berney
[memstalk] SOS wafer
Carl Kubler
2001-12-12
Hello all,

do you know an unexpensive source for 4" Silicon on Sapphire wafers? They
should be backside polished and the thickness of the Si layer should be
around half a micron.

Thank you,
Carl.

----------------------------------------------------------------------
Carl Kubler                                     phone: (604) 291 3481
Physics Department                                fax: (604) 291 3592
Simon Fraser University
Burnaby, BC V5A 1S6
Canada

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
MEMS Technology Review
MEMStaff Inc.