Need for thin film mechanical properties data
1996-06-24
Steve Bolin
Need for thin film mechanical properties data
Steve Bolin
1996-06-24
We are trying to perform mechanical modelling of MEMS devices for theorectical
reliability study. We are currently using bulk mechanical properties of the
materials used in these devices. (Primarily gold, platinum, nickel, silicon and
silicon nitride) Does anyone know of published work giving the mechanical
properties of thin films of these materials?

Thanks,

[email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
MEMStaff Inc.
Nano-Master, Inc.
Addison Engineering