Thick PSG
2001-12-13
Jon Doe
2001-12-14
Michael Pedersen
2001-12-14
Jon Doe
2001-12-14
Michael Pedersen
2001-12-14
Helen Berney
Thick PSG
Jon Doe
2001-12-13
 Hi all:
We are trying to deposit 4 to 10 um thick PSG with 7
to 14 wt% P in a Lam PECVD system. We are experiencing
very high stress and the film cracks and peels of
after an anneal.
Has anybody experience with such thick doped glass
films. If so, How did you overcome the stress?

Thanks for your input.

Thomas

__________________________________________________________________

Gesendet von Yahoo! Mail - http://mail.yahoo.de
Ihre E-Mail noch individueller? - http://domains.yahoo.de

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
University Wafer
Nano-Master, Inc.
Mentor Graphics Corporation