Subject: Silicon emissivity

Does anyone know what the emissivity of silicon is? I know it will be
temperature
dependent, but an idea of the room temperature value would be a good start for
us.

Cheers,

Dave Wood.

-----------------End of Original Message-----------------
there is a table in the Landolt and Bornstein reference books for spectral
emissivity of single crystal silicon at lambda=0.65 um :

T (K) emissivity
1000  0.64
1100  0.62
1200  0.60
1300  0.57
1400  0.54
1500  0.50
1600  0.48
1688  0.46

(Sorry - I've lost the volume number and the reference list, so if you need
anymore info you will need to find a copy of L&B).

-------------------------------------
Shirley Kidner
E-mail: [email protected]

6/25/96
3:12:18 PM

-------------------------------------


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
University Wafer