MEMSnet Home: MEMS-Talk: Hard mask for 20 um deep SiO2 RIE etch?
Hard mask for 20 um deep SiO2 RIE etch?
2001-12-19
[email protected]
2001-12-20
Liz Shelley
2001-12-20
Jon Doe
2001-12-20
[email protected]
2001-12-20
[email protected]
2001-12-20
BERAUER,FRANK (HP-Singapore,ex7)
Hard mask for 20 um deep SiO2 RIE etch?
[email protected]
2001-12-19
We have good results with oxide as a hard mask. Typical selectivities are
>60:1 using oxide. Better than that we have had great results using SU-8 from
Microchem corp. Initial results show a 40:1 selectivity pr:silicon and SU-8
formulations can range from 5-100 microns. It also seems to ash or strip
reasonably well at around 3 microns/minute. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMS Technology Review
Addison Engineering
Mentor Graphics Corporation