glass-glass bonding
Jim Intrater -- IE
2001-12-27
===== Original Message from [email protected] at 12/26/01 6:10 pm
>HI, Does anyone have a detailed protocol for bonding glass to glass? We
>have been trying to bond while maintaining an optical quality surface
>(pure thermal bonding doesn't seem to work) and we haven't had luck with
>applying a voltage across the glass with temp around 400 degrees. We're
>using pyrex right now (borofloat, specifically). Any suggestion would be
>appreciated.
>
>Thanks,
>
>Ziggy
>_______________________________________________
>[email protected] mailing list: to unsubscribe or change your list
>options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
>Hosted by the MEMS Exchange, providers of MEMS processing services.
>Visit us at http://www.mems-exchange.org/
===== Comments by [email protected] ("Jim Intrater -- IE") at
12/27/01 1:32 pm
There are such things as optical adhesives, but they probably won't
withstand 400 degrees.

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Nano-Master, Inc.