MEMSnet Home: MEMS-Talk: surface tension
surface tension
2001-12-29
Yiyi Zhang
2001-12-31
Nickolay V. Lavrik
2001-12-31
Alex Shenderov
2002-01-02
alexander li
2002-01-04
Yiyi Zhang
2002-01-14
Mighty Platypus
surface tension
Yiyi Zhang
2001-12-29
Hi all,
Does anyone know how to significantly decrease surface
tension of photoresists, positive or negative, so as
to spin-coat onto wafers with very low critical
surface tension, such as PTFE? No surface
pre-treatment is allowed because we want to keep the
original low surface energy. Any suggestion is
appreciated.

Thanks in advance.

Yiyi Zhang
Department of Microgravity
Institute of Mechanics, Chinese Academy of Sciences
Beijing 100080
Send your FREE holiday greetings online!
http://greetings.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Tanner EDA by Mentor Graphics
Addison Engineering
Harrick Plasma, Inc.