MEMSnet Home: MEMS-Talk: 110 Si etching with 20%KOH
110 Si etching with 20%KOH
2002-01-04
Connie Kathleen Smith
2002-01-07
Knighton, Ed
2002-01-07
Connie Kathleen Smith
2002-01-07
Knighton, Ed
2002-01-07
Andrew J. Nielson
2002-01-14
Mighty Platypus
110 Si etching with 20%KOH
Connie Kathleen Smith
2002-01-04
I am trying to fabricate a flow channel with vertical side walls using a
<110> Si wafer.  When I etch all the way through the wafer (which is
desired) the side walls are slanted.  The wafers are coated with SiO2 and
Si3N4 as protective barriers during etching.  I expected to lose several
microns vertically during etching but the slanted walls were unexpected.

Thank you,
Connie Smith
Rice University
Department of Chemical Engineering
6100 Main MS 362
Houston, TX  77005

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Nano-Master, Inc.
University Wafer
Addison Engineering