MEMSnet Home: MEMS-Talk: Bonding of quarzt crystal and silicon
Bonding of quarzt crystal and silicon
2001-12-31
wangzy-ime
2002-01-07
[email protected]
Bonding of quarzt crystal and silicon
[email protected]
2002-01-07
I have not done the work myself. I have seen some papers about bonding materials
with differenet thermal expansion properties. In these papers the researchers
have annealed the wafers at low temperature, thinned one of the wafers, then
annealed at high temperature.




"wangzy-ime"  on 12/31/2001 07:47:22 PM

Please respond to [email protected]


To:   [email protected]
cc:    (bcc: Dan W Chilcott/DELCO)

Subject:  [mems-talk] Bonding of quarzt crystal and silicon



Hi, Guys,

Dose any one has experience in bonding single crystalline SiO2(quartz crystal)
onto silicon?  How to overcome the difficulty that their thermal expansion
factors
differ significantly? What is the process? Or, Which papers give detailed
description of the bonding?

Any reply will be greatly appreciated!

Wang, Zheyao
------------------------------------------
Institute of Microelectronics
Tsinghua University
Beijing, 100084 China
Office: Room 3-309
Phone: +86-10-62789147/51 ext. 309
E-mail: [email protected]
        [email protected]
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/




Received: from ahmlir5.mail.eds.com ([205.191.24.45]) by uskokg98.delcoelect.com
(Lotus SMTP MTA v4.6.7  (934.1 12-30-1999)) with SMTP id 05256B35.00538E59; Wed,
2 Jan 2002 10:12:39 -0500
Received: from ahmler3.mail.eds.com (ahmler3.mail.eds.com [192.85.154.74])
     by ahmlir5.mail.eds.com (8.11.6/8.11.3) with ESMTP id g02FChx19855
     for ; Wed, 2 Jan 2002 10:12:44 -0500 (EST)
Received: from kronos.mems-exchange.org (kronos.mems-exchange.org [132.151.8.1])

     by ahmler3.mail.eds.com (8.11.6/8.11.3) with ESMTP id g02F2UE21122
     for ; Wed, 2 Jan 2002 10:02:30 -0500
Received: from localhost ([127.0.0.1] helo=kronos.mems-exchange.org)
     by kronos.mems-exchange.org with esmtp (Exim 3.12 #1)
     id 16LmuM-0003Bq-00; Wed, 02 Jan 2002 10:02:22 -0500
Received: from dns.ime.tsinghua.edu.cn ([166.111.77.2]) by
  kronos.mems-exchange.org with esmtp (Exim 3.12 #1) id 16LD7O-0008EP-00
  for [email protected]; Mon, 31 Dec 2001 19:49:26 -0500
Received: from wandzy ([166.111.233.35]) by dns.ime.tsinghua.edu.cn
  (8.9.2/8.9.2) with SMTP id IAA19962 for ; Tue,
  1 Jan 2002 08:47:35 +0800 (CST)
Message-ID: <[email protected]>
From: "wangzy-ime" 
To: 
MIME-Version: 1.0
Content-Type: text/plain; charset="us-ascii"
X-Mailer: Microsoft Outlook Express 5.00.2615.200
X-Converted-To-Plain-Text: from multipart/alternative by demime 0.98e
X-Converted-To-Plain-Text: Alternative section used was text/plain
Subject: [mems-talk] Bonding of quarzt crystal and silicon
Sender: [email protected]
Errors-To: [email protected]
X-BeenThere: [email protected]
X-Mailman-Version: 2.0.5
Precedence: bulk
Reply-To: [email protected]
List-Help: 
List-Post: 
List-Subscribe: ,
     
List-Id: General MEMS discussion 
List-Unsubscribe: ,
     
List-Archive: 
Date: Tue, 1 Jan 2002 08:47:22 +0800


|--------------------------------------->
|USKOKG98/us/delphiauto                 |
|USKOKH99/us/delphiauto                 |
|USKOKHM1/DELCO                         |
|USKOKM08/DELCO                         |
|--------------------------------------->
  >---------------------------------------|
  |01/02/2002 10:12:41 AM - 01/02/2002    |
  |10:12:42 AM                            |
  |01/02/2002 10:12:47 AM - 01/02/2002    |
  |10:12:56 AM                            |
  |01/02/2002 10:12:51 AM - 01/02/2002    |
  |10:13:34 AM                            |
  |01/02/2002 10:13:34 AM - 01/02/2002    |
  |10:13:35 AM                            |
  >---------------------------------------|

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMStaff Inc.
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.