A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: RE: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
Re: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
2002-01-10
Victor Lifton
RE: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
2002-01-10
Art Glidden
RE: FW: [mems-talk] Non-Chromium Trioxide Defect Etch
Art Glidden
2002-01-10
"MEMC Etch-A Chromium Trioxide-Free Etchant for Delineating Dislocations and
Slip in Silicon" Journal of the Electrochemical Society, Solid-State Science
and Technology, March 1990

(Sorry if the reference format is non-standard)

Thanks for your interest,

A.G.

-----Original Message-----
From:   [email protected] [mailto:[email protected]] On
Behalf Of Victor Lifton
Sent:   Thursday, January 10, 2002 10:32 AM
To:     [email protected]
Subject:        Re: FW: [mems-talk] Non-Chromium Trioxide Defect Etch

Would you please send me a reference to that MEMC
paper.
Thank you,
VL

> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On
> Behalf Of Art Glidden
> Sent: Thursday, January 10, 2002 8:20 AM
> To: [email protected]
> Subject: [mems-talk] Non-Chromium Trioxide Defect
> Etch
>
>
> Looking for a non-CrO3 etch for finding dislocation,
> slip, and stacking
> fault defects in 100 Si slices. I've read a 1990
> paper on an etch employing
> Copper Nitrate, developed at MEMC. Experience using
> that, or other, more
> user-friendly etchant for this purpose?
>
> A.G.
> _______________________________________________
> [email protected] mailing list: to unsubscribe
> or change your list
> options, visit
>
http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS
> processing services.
> Visit us at http://www.mems-exchange.org/
Send FREE video emails in Yahoo! Mail!
http://promo.yahoo.com/videomail/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
MEMS Technology Review