A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: nitride to Si bonding?
nitride to Si bonding?
2002-01-09
Nickolay V. Lavrik
2002-01-10
Kenneth Smith
2002-01-10
Heiko van der Linden
2002-01-10
Roger Shile
2002-01-11
Niels Olij
nitride to Si bonding?
Kenneth Smith
2002-01-10
I understand that the same fusion bonding that is done with SOI wafer
using oxide can be done with a nitride layer. Suggest contact
http://www.affixtek.com as I know they were working on this.


Regards,
Ken

Nickolay V. Lavrik wrote:

> I know that standard bonding processes are
> available for materials such as Si, oxide and
> pyrex.
>
> Does any one if similar procedures exist for
> reliable (without organic adhesives) permanent
> bonding of Si and nitride coated wafers.
>
>
> Any relevant information will be highly
> appreciated
>
> Nickolay
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
>
>


--


Kmbh Associates
4968 Charter Road
Rocklin, CA  95765  U  S  A
510-714-5055 Efax- 510 217 4421 or 561 658 6136

High Purity Float Zone and Specialty CZ Silicon  for Power, IR and
Mirror Optics, Optoelectronics, MEMS, SOI, and other Semiconductor
applications. Service in SOI, Polishing SSP and DSP.
Quartz, Glass, Pyrex and Borofloat Wafer Supply. Anodic Bonding. SOG, SOS.
Email me for current excess stock of SI and SOI Wafers Available- 11,000
Stock

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Addison Engineering
The Branford Group
Mentor Graphics Corporation
Process Variations in Microsystems Manufacturing