Hi Nickolay,

if you have to make the nitride wafer silicon  anodic bonding with silicon
you must growth SiO2 on nitride wafer with high percentage of Na.


Greets,
Luciano Scaltrito
----------------------------------------------------------------------------
------------
Ing. Luciano Scaltrito
Dipartimento di Fisica
Politecnico di Torino
C.so Duca degli Abruzzi, 24
10129 Torino, Italy
tel +39 011 564.7305/564.4160
fax +39 011 564.7399
E-mail : [email protected]
http://www.polito.it/centri/laborato/limadel/film/index.html
----------------------------------------------------------------------------
------------

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Nano-Master, Inc.
Harrick Plasma, Inc.
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics