Warner,

A special thanks from me for your input.

roger brennan

-----Original Message-----
From:   Venstra, W.J. [SMTP:[email protected]]
Sent:   Thursday, January 10, 2002 7:15 AM
To:     '[email protected]'
Subject:        RE: [mems-talk] Si crystal

Hello Hauke,
You might find following link useful:
http://bsac.eecs.berkeley.edu/~pister/crystal.pdf
Regards,
Warner


________________________________________________________________
Warner J. Venstra
Delft University of Technology
Department of Mechanical Engineering


> -----Original Message-----
> From: Hauke Schuett [SMTP:[email protected]]
> Sent: Thursday, January 10, 2002 12:52 PM
> To:   [email protected]
> Subject:      [mems-talk] Si crystal
>
> Hello,
> is there someone out there who can provide some kind of illustration of
> the
> cristall lattice of Si?
> Further, and the main focus, where are which crystal planes and why are
> the
> etchants so selective at these directions? (you see I start at the very
> beginning)
>
> Thanks for your help!
>
> Hauke
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Addison Engineering
Mentor Graphics Corporation