Can anyone suggest an optically transparent adhesion (tie) layer that can be
used between a vapor deposited silver film and a glass substrate?  We would
normally use titanium or chrome, but in this application we need optical
transparency.

Thanks,

Timothy A. Postlethwaite, Ph.D.
Principal Scientist
Constellation Technology Corporation
7887 Bryan Dairy Road, Suite 100
Largo, Florida 33777
(727) 547-0600 x 6177
(727) 545-6043 (fax)
[email protected]
http://www.contech.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
MEMS Technology Review
Harrick Plasma, Inc.
Addison Engineering