Polyimide processing
2001-07-28
gururaj shenoy
Polyimide processing
gururaj shenoy
2001-07-28
Hello all

I am trying to pattern polyimide on silicon nitride wafers. When i dispense
the polyimide on the wafer and spin it for the required thickness i find the
polyimide shrinking from some areas of the wafer and morae and more
shrinking of the polyimide taking place within a minute of spinning.

Also i would like to know if anyone has an optimum recipe for the dispensing
and treating polyimide.

Also i want to know how we can bond two patterned polyimide back to back  (
whether it can be done after curing or should it be packed back to back and
cured with heating). Does any one know how to do bonding of polyimide.

Help in this regard would be greatly appreciated.

Thanx

Gururaj Shenoy
Lousiana Tech University

_________________________________________________________________
Get your FREE download of MSN Explorer at http://explorer.msn.com/intl.asp



reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Addison Engineering