Dear All,

I have been using a microwave asher to remove hardened resist after RIE
etching.  I tried to remove some resist residue recently on a 6" wafer that
had 1um of Cr deposited on it.  I used the following parameters 600ml/min
oxygen which gives about 0.8 bar and 600W power for 60mins.  I found that
the Cr had been etched and re-deposited all over the inside of the chamber
as CrOx (i think it could be) ! Does anyone have any idea about how this
might have happened ? My theory is that the microwaves have coupled into to
the wafer and increased the surface temperature.

many thanks,

Iain Watson.


********************************************************************
This email and any attachments are confidential to the intended
recipient and may also be privileged. If you are not the intended
recipient please delete it from your system and notify the sender.
You should not copy it or use it for any purpose nor disclose or
distribute its contents to any other person.
********************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
The Branford Group
Mentor Graphics Corporation