Jean Podlecki
2002-01-24
This can be usefull

http://www.uoregon.edu/~hutchlab/semilab/etchants.pdf

Jean.

-----Original Message-----
From: Andrew Dowling [mailto:[email protected]]
Sent: Wednesday, January 23, 2002 9:31 PM
To: [email protected]
Subject: Re: [mems-talk] Visit to the Library


Deleted, happily.

My mother once said to me, "Be constructive or be quiet". You won't find
this
in a library!



>>> [email protected] 01/23/02 07:19AM >>>
Dear All,

Of late it has been my observation that some people have stopped visiting
library and rely on the MEMS mailing list for information for their grad
projects. I think the purpose of this list is to share experience and
discuss show stoppers in the FAB or design not just to save a trip to the
library. So I strongly feel that questions like below answers to which can
be found
in any (thin film) text book,  should be discouraged.

Regards
Amit

Tao YU wrote:

> Hi, friends,
>
> Could anyone tell me how to wet-etch Cr/Au films? Which etchant should I
> use? Thanks.
>
> Tao YU
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/





"Your reality is a figment of my Imagination"
      ......... To me you exist because I imagine that you do.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/


**********************************************************************
The information in this email and any attachments is strictly confidential and
is intended for the addressee only. Access to this email by any other person is
unauthorised. If you are not the intended recipient please destroy this message,
delete any copies held on your systems and notify the originator immediately by
reply email.  The unauthorised use, disclosure, copying, lteration, distribution
or any action taken or omitted to be taken in reliance of this email is strictly
prohibited and may be unlawful.
Addressees should scan all attachments (if any) for viruses. This email
and any attachments have been scanned for viruses prior to leaving the
Alcatel Optronics network.  Please note that neither Alcatel Optronics nor the
sender will accept responsibility or be liable for any direct, indirect or
consequential damages arising from any alteration to the contents of
this email by a third party or as a result of any virus being passed on.
Opinions and views expressed in this email are those of the sender.
They may not reflect the opinions and views of Alcatel Optronics and shall be
understood as being neither given nor endorsed by it.

**********************************************************************

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing
Addison Engineering