That's Aqua Regia.  One metal that is not etched by this combination is
Chrome.

David Nemeth
Senior Process Engineer
Sophia Wireless, Inc.
14225-C Sullyfield Circle
Chantilly, VA
Ph: (703) 961-9573 x206
Fax:(703) 961-9576

-----Original Message-----
From: [email protected] [mailto:[email protected]]On
Behalf Of Rivas, Isabel
Sent: Thursday, January 24, 2002 11:26 AM
To: '[email protected]'
Subject: [mems-talk] metal resistant to HCl:HNO3


Hello,

Could anyone tell me a metal which resists this etchant: HCl:HNO3 (8:1)?

Thank you very much

         Isabel.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
The Branford Group
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation