MEMSnet Home: MEMS-Talk: Re: Metal sticking well to silicon and silicon nitride
Re: Metal sticking well to silicon and silicon nitride
1996-07-03
Mac McReynolds
1996-07-03
[email protected]
1996-07-04
Nutt Wolfgang
1996-07-04
Pierre Jaccard
1996-07-05
Padmaja Ramadas
1996-07-09
Bahram Ghodsian
1996-07-10
Mac McReynolds
1996-07-17
[email protected]
Re: Metal sticking well to silicon and silicon nitride
Nutt Wolfgang
1996-07-04
Xuecheng Jin wrote:
>
> May I know what kind of good conducting metal stuck well to silicon wafer
> and silicon nitride thin film? How about gold? Do we need to put interface
> layer such as cromium etc. to get better adhesion? Thanks a lot.
>
> Best Regards.                                            Sincerely Yours,
>                                                          XueCheng JIN
>
>
>

We used gold as a masking material on oxid- and nitrid-wafer. Chromium
(Sputter) or Nickel (Evaporation) were good interface layers.

Yours,

W. Nutt
--

                                         __\/__
                                     .  / ^  _ \  .
                                     |\| (o)(o) |/|
 -------------------------------|-.OOOo----oo----oOOO.-|------------
 NEU-TECHNIKUM BUCHS            |                      |
 Wolfgang Nutt, Faching. NTB    |           (c)remund  |
 Transferassistent IMS          |                      |
 CH-9471 Buchs                  |___________Oooo.______|
 Phone: +41 81 755 34 49             .oooO  (   )
 Fax:   +41 81 756 54 45             (   )   ) /
                                      \ (   (_/
 eMail: [email protected]                    \_)

 WWW:   http://www.ntb.ch/Intern/Assistenten/nu.html

 PGP Public Key aviable.


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Mentor Graphics Corporation
Harrick Plasma, Inc.
Nano-Master, Inc.