polyimide stripper?
2002-01-31
apatel43
2002-01-31
Michael Martin
2002-01-31
Mac McReynolds
2002-01-31
Walter Stonas
2002-01-31
[email protected]
2002-01-31
BERAUER,FRANK (HP-Singapore,ex7)
2002-02-01
Rivas, Isabel
2002-02-01
Michael Martin
2002-02-04
Rivas, Isabel
2002-02-04
[email protected]
polyimide stripper?
Mac McReynolds
2002-01-31
Try Shipley Microposit 1165 (NMP)

Mac McReynolds
R&D Manager
Caliper Technologies Corp.
605 Fairchild Drive
Mountain View, CA 94043-2234
Tel:  650-623-0710
Fax:  650-623-0521

> ----------
> From:         apatel43
> Reply To:     [email protected]
> Sent:         Thursday, January 31, 2002 8:42 AM
> To:   [email protected]
> Subject:      [mems-talk] polyimide stripper?
>
> Hi,
>
> I was wondering if anyone knows of a photoresist stripper which would take
> off
> a polyimide layer?
>
> Thanks,
> Arti Patel
>
> Arti Patel
> Research Assistant/Graduate Student
> University of Illinois at Chicago
> Department of Bioengineering
> 851 S. Morgan St. (m/c 063)
> Chicago, IL 60607
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review