Bob,
    yes I think it does: its response time is 3-5 ms; its chip measures 1.5 x
1.5 x 0.5 mm and its velocity measurement range is typically 1 to 1000 cm/s.
Its commercial package includes an electronic circuit on a 25 x 25 mm alumina
substrate. Cost: 40-80$ depending on quantity. Model No.: AWM4000, designed
for the user to provide his own flow channel. I assume it is larger than 25
mm diameter?
Ulrich
_______________________________________________________________________________
From: Horning Bob on Mon, Jul 1, 1996 9:24 AM
Subject: FW: MEMS flow sensors
To: Bonne Ulrich

Ulrich

Does our MAF sensor fit this description?

Bob
_______________________________________________________________________________
From: [email protected] on Fri, Jun 28, 1996 8:18 PM
Subject: MEMS flow sensors
To: [email protected]

Hi,


  I am looking for a directional flow sensor which has a response time on the

order of milliseconds and comes in a small package (< 2 mm).  It has to work
in
a high flow ambient, say 4 liters/sec, but does not have to quantitatively
measure the flow, just sense directional changes.  Does anyone know of any
existing products.  Thanks for your time.


Sincerely,


John Buan

John S. Buan
Minnesota Innovative
     Technologies and Instruments Corp.
603 Washington Ave. SE  #503
Mpls., MN 55414-2950
[email protected]
phone: (612) 626-1541
fax:   (612) 625-0558



------------------ RFC822 Header Follows ------------------
Received: by msmail.htc.honeywell.com with SMTP;28 Jun 1996 20:17:58 -0600
Received: from darkstar.isi.edu by cams.htc.honeywell.com; Fri, 28 Jun 96
20:18:10 CDT
Received: by darkstar.isi.edu (5.65c/5.61+local-23)
        id ; Fri, 28 Jun 1996 17:31:32 -0700
Received: from venera.isi.edu by darkstar.isi.edu (5.65c/5.61+local-23)
        id ; Fri, 28 Jun 1996 17:31:30 -0700
Received: from darkstar.isi.edu by venera.isi.edu (5.65c/5.61+local-23)
        id ; Fri, 28 Jun 1996 17:31:29 -0700
Received: by darkstar.isi.edu (5.65c/5.61+local-23)
        id ; Fri, 28 Jun 1996 17:31:28 -0700
Message-Id: <[email protected]>
From: "John S. Buan" 
Subject: MEMS flow sensors
Date: Thu, 27 Jun 96 11:21:31 -0500
To: [email protected]
X-Url: http://mems.isi.edu/mems.html
Reply-To: [email protected]


reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Nano-Master, Inc.
The Branford Group
MEMStaff Inc.