Jennifer Scalf
2002-02-03
shay kaplan
2002-02-03
li gang
2002-02-04
Inna
2002-02-06
Burkhard Volland
HMDS: is it really that bad?
shay kaplan
2002-02-03
Dear Jennifer,
Way back,HMDS was widely used as a 10-20% solution in EGMEA wich was the
positive resist solvent. The fumes of both together was reported to cause
some health problems and was not reccomended for pregnant women. I tend to
think that when the industry moved to PGMEA 'safe solvent' the problem went
away.

Shay

Jennifer Scalf wrote:

> I've heard from many people that HMDS is very, very bad for you.
> However, the few MSDSs that I have read do no indicate that it is
> anything other than a strong irritant and highly flammable.  Why do
> people seem to think it is a teratogen, mutagen, carcinogen, etc?  Do
> some MSDS's have more information than others?  If so, can someone point
> me toward one that explains hazards other than irritation and
> flammability.
>
> Jennifer
> _______________________________________________
> [email protected] mailing list: to unsubscribe or change your list
> options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
> Hosted by the MEMS Exchange, providers of MEMS processing services.
> Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Tanner EDA by Mentor Graphics
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.