I was extremely dissatisfied with the service I got from Photronics after they
took over Micromask.  I asked for a clear field mask.  What they gave me had a
chrome border that ran into and was contiguous with my features, rendering the
mask useless.  When I complained I was told something to the effect that the
mask was made my specifications.  Further calls went unanswered.

Photronics apparently has a different definition of "clear field" then the
former Micromask, or any other mask maker I have used since.

Since the demise of Micromask, I have been using Photo Sciences for my high
resolution photomasks and have been very happy with their service.

For inexpensive lower resolution masks I would recommend HTA Photomask.

>>> [email protected] 02/01/02 02:19AM >>>
Hi Yong,

Photronics MZD is a photomaskprovider.
E-mail: [email protected]

Regards

Miriam



--------------------------------------------
SUSS MicroTec
Applications Center Europe
Miriam Bruckner
Schleissheimer Str. 90
85748 Garching
Germany
Fon     +49 89 32007 - 385
Fax     +49 89 32007 - 390
email   [email protected]



-
Message: 6
From: "Yong Zhu" 
To: 
Date: Thu, 31 Jan 2002 01:28:24 -0600
Subject: [mems-talk] photomask company with 1 micron CD
Reply-To: [email protected]

Dear All,

I am looking for a photomask company which can supply with 1 micron Critical
Dimension.
Any information will be highly appreciated.

Regards,

Yong

--__--__--
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Harrick Plasma, Inc.
Nano-Master, Inc.
Tanner EDA by Mentor Graphics