    I am doing the resistivity measurements of  Cu
films
deposited on Si substrate with native oxide by van der

Pauw  method.While calculating  Rho I have some
concussion regarding the thickness...Whether I have to
use the  wafer + film  thickness or only the film
thickness. Please gave some reference regarding this..
     Thanks in advance
                                    Sinu Mathew
Send FREE Valentine eCards with Yahoo! Greetings!
http://greetings.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
Nano-Master, Inc.
Process Variations in Microsystems Manufacturing