We are doing some work on microhotplates and have been running a
simulation in MEM CAD. I have noticed a degree of variation in the
charge density near corners in the hot plate.

-Mike

>>> [email protected] 02/04/02 10:44AM >>>
Hi all,

I'm doing some heat transfer numerical simulation of a thinfilm heater
that
has a lot of 90-deg turns. The heater is made of evaporated gold on a
single crystal LSN substrate. The dimension is 400um wide and about 1um

thick, and I'm applying a 5-15VDC current-unlimited power to the
heater. I
understand that the method of fabrication might have introduced some
thickness non-uniformity at the corners. But if I assume the thickness
is
uniform, is electrical conduction at corners differ noticeably than for
a
straight path (like in fluid flow)? Or does the electron spatial and
temporal scale of travel make the existent of the corner irrelevant?

Any suggestions and/or references would be greatly appreciated.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk

Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics