A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Shadow Masks
Shadow Masks
2002-02-06
Nirmal Govindaraju
2002-02-07
Klauder, Jr., Philip R.
2002-02-07
David Nemeth
2002-02-07
Barry Wissman
2002-02-11
Bigelow . Mike
Shadow Masks
Barry Wissman
2002-02-07
Try a place in Chicago called FotoFab (www.fotofab.com). They can do wet
chemical etching of photolithographically patterned stainless steel. I would
try a stainless thickness of ~ 0.005" (125 um), which should be a good
compromise between rigidity and machinability. Note that the minimum feature
size is proportional to the thickness.
___________________________________________
Message: 8
Date: Wed, 6 Feb 2002 11:27:44 -0500 (EST)
From: Nirmal Govindaraju 
To: 
Subject: [mems-talk] Shadow Masks
Reply-To: [email protected]

Hi,

I'm a Graduate Student at North Carolina State University and I am looking
for some information on people who produce shadow masks. Please note that
I will be using the shadow masks to fabricate thin film resistors and
thermocouples on a substrate using e-beam evaporation.

Thank you.
Sincerely,
Nirmal Govindaraju

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
The Branford Group
MEMStaff Inc.
Process Variations in Microsystems Manufacturing
MEMS Technology Review