Jamie Wang
2002-02-08
[email protected]
Dry release
[email protected]
2002-02-08
I don't know who makes a system anymore but there is a way to etch release
oxide layer using vapor HF system. Another shot might be to use a downstream
isotropic etch tool like a Matrix or Ulvac and do it in a plasma. This
depends on the feature size you are trying to release. If it is too big
compared to the thickness of oxide you are removing it probably won't work
well. Bob Henderson

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
Harrick Plasma, Inc.
Process Variations in Microsystems Manufacturing