Hi,

I have 8 um width,  15 um deep channels anisotropic etched in SiO2 and want
expose in a positive photoresist 3 to 6 um width lines on the bottom of
this channels. Have anybody ever tried something similar? I have problems
with optical lithography (proximity effects), so am thinking on E-Beam
lithography... Can one positioning a sample in REM without simultaneously
significant exposing the resist? There are different PMMA types (and others
resists?), what would be most suitable? Would it works at all?

Regards,
Evgeny Gutyrchik

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
MEMS Technology Review
Mentor Graphics Corporation
MEMStaff Inc.
Harrick Plasma, Inc.