A MEMS Clearinghouse® and information portal
for the MEMS and Nanotechnology community
RegisterSign-In
MEMSnet Home About Us What is MEMS? Beginner's Guide Discussion Groups Advertise Here
News
MEMSnet Home: MEMS-Talk: Ultra-thick Electrodeposited Resists
Ultra-thick Electrodeposited Resists
2002-02-14
Whye-Kei Lye
2002-02-19
BERAUER,FRANK (HP-Singapore,ex7)
Ultra-thick Electrodeposited Resists
BERAUER,FRANK (HP-Singapore,ex7)
2002-02-19
Hi YK,

In theory, electrophoretic resist deposition is a self-limiting
process and the thickness depends solely on the voltage. But we
found that time (and various other parameters not fully under-
stood yet) also play a role.
We achieved PEPR thickness of 10-30um at 100-200V. In a watery
bath I personally would't dare to apply much higher voltages.
Consistent thickness control is difficult and we found that a
good recirculation system and a well-kept bath is very important.
Some components also evaporate over time and need to be topped
up if you keep the bath over long periods (At the price of PEPR,
chances are you have to).
Shipley and Semitool (they are developing a plating bath for
PEPR, which gives MUCH better results than our modified metal
plating bath or any desktop beaker setup) are helpful and you
can also contact them.
Please reply to me directly if you would like a more detailed
discussion.

Greetings,
        Frank Berauer
        Senior R&D Engineer
        Hewlett-Packard Singapore


-----Original Message-----
From: Whye-Kei Lye [mailto:[email protected]]
Sent: 15 February 2002 05:50
To: [email protected]
Subject: [mems-talk] Ultra-thick Electrodeposited Resists


Hi all,

I am looking to use Shipley's PEPR 2400 electrodeposited positive resist
for making 200 - 200 micron thick coatings.  Does anyone know if this is
possible/realistic?  What sort of thicknesses are possible with this
resist?

Any insight would be greatly appreciated.

Thanks in advance,

yk

____________________________________________________________________________
__

Whye-Kei Lye, Ph.D.
Research Scientist
Department of Electrical and Computer Engineering
University of Virginia
434-982-2374
[email protected]
____________________________________________________________________________
__
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Mentor Graphics Corporation
Tanner EDA by Mentor Graphics
The Branford Group
Harrick Plasma, Inc.