2002-02-18
[email protected]
2002-02-18
C. Suzanne Miller
Making metal clusters on Si substrate
2002-02-19
Junghoon Yeom
2002-02-18
Rohit Srivastava
2002-02-18
Jon Doe
2002-02-19
Liz Shelley
2002-02-19
Blunier, Stefan
2002-02-19
[email protected]
2002-02-19
[email protected]
2002-02-19
[email protected]
Positive resists for MEMS processing
[email protected]
2002-02-19
Have you had problems with SU-8 on your drie? What type of problem? We
haven't seen any problems to date even when we switch back and forth from
positive resist to SU-8. Do you have the capability of coating 10 wafers with
the Shipley resist using a MEMS type mask with 2-50 micron trenches on 4"
wafers? Gladly pay for such samples. Bob Henderson 480-558-1156

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
Addison Engineering
Mentor Graphics Corporation
The Branford Group