Bill Moffat
RE: mems-talk digest, Vol 1 #201 - 9 msgs
Bill Moffat
2002-02-22
Yes there are at least 2 commercial mask aligners that will align both sides
of the wafer O.A.I. and Quintel.  Microchem is the company with the
photoactive compound NANO MX 6C there was a question about yesterday, phone
number 617 965 5511 a good contact is Mark Shaw ext. 308.  The same company
may have the answer for thick Polymide.  The thickest I have worked with is 80
microns of Polymide but I have worked with 400 micron thick SU8 a negative
acting chemically amplified resist produced by Microchem.  Plasma experiments
on bridge structures can be done using my companies horizontal/vertical
plasma, it is designed to sweep under bridges, if I am contacted.  Bill
Moffat

-----Original Message-----

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Harrick Plasma, Inc.
MEMStaff Inc.
MEMS Technology Review