MEMSnet Home: MEMS-Talk: Etchant for Cr
Etchant for Cr
1996-07-16
Behrouz Nikpour
1996-07-17
Alexander Holke
Etchant for Cr
Alexander Holke
1996-07-17
You can use any comercial Cr etchant used in mask fabrication.
HCl, let's say 10%, works if you touch the Cr with a less noble
metal (Al works fine). The electrochemical voltage dissolves the
oxide on the Cr which protects it initially. "Magic Touch" it is
also called.

Alexander Hoelke