Hi,
actually http://aveclafaux.freeservers.com/SU-8.html#top has the breakdown
voltage... since today :-) (actually it was discussed on the list some weeks
ago)
1.1 10^5 V/m from the measurement of Jim Thorpe
.
You may try to contact him, he may have measured the conductivity before the
breakdown :-)
Franck

"-----Original Message-----
"From: Ohnstein, Tom (MN14) [mailto:[email protected]]
"Sent: Thursday, 28 February, 2002 06:21
"To: '[email protected]'
"Subject: [mems-talk] Electrical Properties of SU-8
"
"
"I am looking for information on the electrical properties of SU-8,
"specifically electrical conductivity and electrical breakdown
"strength.  I
"have already spoken with Microchem and they had no information on these
"properties.  On the web site that is compiling all information known to
"mankind on SU-8, they had dielectric constant but that was
"about all for
"electrical properties. Does anyone have any data on electrical
"conductivity/resistivity and electrical breakdown strength?
"
"Thanks
"
"
"Thomas Ohnstein
"Principal Scientist
"Honeywell Laboratories
"[email protected]
"_______________________________________________
"[email protected] mailing list: to unsubscribe or change your list
"options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
"Hosted by the MEMS Exchange, providers of MEMS processing services.
"Visit us at http://www.mems-exchange.org/
"

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
Addison Engineering
Harrick Plasma, Inc.
Tanner EDA by Mentor Graphics