Anodic bonding glass-titanium
2002-03-01
[email protected]
2002-03-01
Abhinav Bhushan
2002-03-01
Islam Rafiqul
2002-03-01
Roger Shile
2002-03-02
Antonius Helvoort
2002-03-05
Niels Olij
Anodic bonding glass-titanium
Roger Shile
2002-03-01
I tried unsucessfully to bond Pyrex to a chrome film in air.  However someone
on this forum indicated they were able to do this in a nitrogen ambient.

I understand that many metals can be andoically bonded to Pyrex.  The trick
may be to prevent excessive oxidation of the metal during bonding.

Roger Shile



>>> [email protected] 03/01/02 02:06AM >>>
I tried to make anodic bonding between glass and titanium but it was
unsuccessful.  Have you any idea about why it didn't succeed ?

Thank you in advance.
_______________________________________________
[email protected] mailing list: to unsubscribe or change your list
options, visit http://mail.mems-exchange.org/mailman/listinfo/mems-talk
Hosted by the MEMS Exchange, providers of MEMS processing services.
Visit us at http://www.mems-exchange.org/

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
University Wafer
MEMStaff Inc.
The Branford Group
Addison Engineering