Hi,
        Right now we're using chrome-gold-chrome layers, 100A-150A-100A to
protect for glass etching. I noticed that if I do a BOE etch over 35
minutes, it starts to eat through the layers some and makes the channel
edges rough. I wondered if, in addition to thicker protective layers, the
preparation of the glass surface had an effect, say a SC-1/BHF clean
instead of H202:H2SO4.

THanks,

Ziggy

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Harrick Plasma, Inc.
MEMS Technology Review
Addison Engineering
MEMStaff Inc.