Anodic bonding glass-titanium
2002-03-01
[email protected]
2002-03-01
Abhinav Bhushan
2002-03-01
Islam Rafiqul
2002-03-01
Roger Shile
2002-03-02
Antonius Helvoort
2002-03-05
Niels Olij
Anodic bonding glass-titanium
Abhinav Bhushan
2002-03-01
can you divulge some details of the process?
temperature, thickness of Ti layer, cleaning method,
time, force, contact area, glass type...

Abhinav

--- [email protected] wrote:
> I tried to make anodic bonding between glass and
> titanium but it was unsuccessful.  Have you any idea
> about why it didn't succeed ?
>
> Thank you in advance.
Yahoo! Greetings - Send FREE e-cards for every occasion!
http://greetings.yahoo.com

reply
Events
Glossary
Materials
Links
MEMS-talk
Terms of Use | Contact Us | Search
MEMS Exchange
MEMS Industry Group
Coventor
Harrick Plasma
Tanner EDA
Process Variations in Microsystems Manufacturing
Mentor Graphics Corporation
MEMS Technology Review
Tanner EDA by Mentor Graphics